论文部分内容阅读
1前言本研究旨在对不同钻含量(约3%~13%)和不同碳化钨晶粒度的中低钻合金的电溶速度、工艺参数作一些比较,以求发挥设备和资金的最佳效能。2实验方法2.1选取各种刀片和合金碎片,每种约skg,装入电解槽的阳极盒中,每个阳极盒的两边均安装有阴极板,在1.5~1.6V直流电
1 Preface The purpose of this study is to make some comparisons of the elec- trolytic speed and process parameters of medium and low-alloy alloys with different diamond contents (about 3% ~ 13%) and different tungsten carbide grain sizes in order to make the best use of equipment and capital efficacy. 2 Experimental Methods 2.1 Select a variety of blades and alloy fragments, each about skg, into the anode tank cell, each anode box is installed on both sides of the cathode plate at 1.5 ~ 1.6V DC