论文部分内容阅读
1 配方 亚氯酸钠25%+氧化锌10%+硫酸亚铁15%+活性炭50%。2 配制 将上述4种药剂按比例混合均匀,加少许水充分搅拌,在110℃下干燥,研磨成直径2.5mm的颗粒。
1 formula sodium chlorite 25% + zinc oxide 10% + ferrous sulfate 15% + activated carbon 50%. 2 Preparation The above four kinds of pharmaceutical agents are mixed in proportion, with a little water and stir, dried at 110 ℃, ground into 2.5mm diameter particles.