mm坯连铸相关论文
在分析37Mn5钢(/%:0.34~0.39C,0.20~0.35Si,1.25~ 1.50Mn)凝固特性的基础上通过用ANSYS软件建立连铸圆坯凝固热-力耦合数学模型,对Φ210 m......
生产的高压锅炉用钢SA-210A1(/%:0.08~0.11C,0.22~0.24Si,0.72~0.74Mn,0.007~0.010P,0.004~0.005S,0.010~0.015V,0.025~0.035Ti,0.012~0.018A......