专利申请号:CN201110347902.9公开号:CN102398920A申请日:2011.11.07公开日:2012.04.04申请人:北京航空航天大学一种射流空化技术制备二维纳米二硫化钼的方法,它有七大步骤:(1)按重量比将二硫化钼粉等三种原料配制成二硫化钼水溶液放入储料罐中;(2)二硫化钼水溶液由储料罐进入柱塞泵加压至指定压力;(3)二硫化钼水溶液进入空化发生器中发生片
Patent application CN201110347902.9 Publication Number CN102398920A Application date: 2011.11.07 Published date: 2012.04.04 Applicant: Beijing University of Aeronautics and Astronautics A method for preparing two-dimensional nano-molybdenum disulfide by jet cavitation technology, which has seven major Step (1) according to the weight ratio of three kinds of raw materials such as molybdenum disulfide powder formulated into an aqueous solution of molybdenum disulfide into the storage tank; (2) molybdenum disulfide solution from the storage tank into the plunger pump to the specified pressure ; (3) molybdenum disulfide aqueous solution into the cavitation generator occurred tablets