本文介绍了局部芯体人为裸露的 U_3Si_2-Al 弥散型燃料板水煮腐蚀试验。结果表明,不仅水中没有发现铀,而且裸露芯体的显微结构也无明显变化。
This paper introduces the boiled corrosion test of U_3Si_2-Al dispersed fuel plate with local core exposed by human. The results showed that not only uranium was not found in water, but also the microstructure of bare core did not change significantly.