150吨纯氧顶吹转炉采用四孔喷枪吹炼过程温度的变化

来源 :鞍钢技术 | 被引量 : 0次 | 上传用户:marsmoonhoo
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
顶吹转炉吹炼过程的温度控制,是操作中心环节之一。温度对于熔池化学反应进行的速度有决定性的意义。炼钢工作者都在竭力摸索转炉吹炼过程温度的变化规律。连续测温攻关小组与三炼钢厂的工人、干部、技术人员互相配合,共同在150吨转炉进行了炉衬埋入热电偶连续测温的现场试验,取得了一定成绩。本文根据连测结果,对转炉吹炼过程中的钢液温度和炉衬 Top blowing converter blowing temperature control process, is one of the operational links. The temperature is of decisive importance for the speed of the chemical reaction in the bath. Steel-making workers are trying their best to find out the change rule of the temperature in converter blowing process. Continuous temperature measurement team and the third steel mill workers, cadres and technicians work together in a 150-ton converter furnace lining embedded thermocouple continuous temperature field test and achieved some success. In this paper, according to the results of continuous measurement, the temperature of the molten steel during the converter blowing and lining
其他文献
钙硅渣是多相材料,含有75~80%的3CaO·Al_2O_3·xSiO_2·(6~2x)H_2O型的钙水化石榴石(分子式中的x由于脱硅方法的不同而为0.15~0.25);10~15%的含水碳铝酸钙 Calcium silicate sla
“新买的一部手机,开机后就一直呈‘冻机’状态,既不能打电话也不能接听,所谓的准智能手机成了一部模型。”近日,吉林的赵女士向媒体投诉江西风尚电视购物中心。10月26日,赵
高炉炼铁实践证明,风温每提高100℃,产量可提高4~3%,焦比可降低4~3%。可见提高风温是降焦增铁的有效措施之一。提高风温的途径,除改进热风炉结构和改善热风炉操作外,对小高炉来
近年来,我国在强磁机的研制方面,出现了多种类型的强磁机,在解决弱磁性矿物的选矿问题上,取得了很大进展。但从已有的类型看,大多数是用于细粒嵌布的矿物,而适用于中等粒级
一、矿石性质易门老厂钴土矿属风化残留矿床,矿体赋存于白云岩风化层内。矿石中主要脉石矿物为石英及少量白云岩、方解石、云母、粘土等。脉石矿物量75~77%。矿石中金属矿物
为了提高生产效率,要求运行电解槽具有稳定的侧部槽帮。电解槽热平衡的变化可以使侧部槽帮凝固和熔化,而根据槽帮厚度的大小来调节电解槽的能量输入,在理论上可以将这种凝固
使用普通的直拉法生产单晶硅将形成大量氧复合体。高温处理硅时,这些氧杂质的存在能导致各种各样的晶体缺陷。然而,通过精心的控制热处理过程,就能够控制氧的沉淀量,从而最终
一、前言为获得竖炉焙烧赤铁矿球团的良好指标,我们在生球进炉焙烧前采用了“钢网带干燥机”这一手段,用以对生球进行脱水、干燥。虽然试验时间不长(仅一个月),而且也发现某
多吃废钢铁,降低铁钢比是节能的一个重要措施。我国许多设备将更新换代,可提供一定量的废钢资源。 例如,浙江省每年将有20万吨废钢。世界航运不景气,旧船价格极低,拆旧船炼
前三讲介绍了对象特性、测量元件和执行机构的特性。现在介绍调节器的作用、类型、特性及其对调节质量的影响。目前,广泛使用的调节器主要有两位、比例、积分、微分调节作用