论文部分内容阅读
最早组织工业生产蒸压粉煤灰砖的是西德。在一家电厂区建成了一座日产九万砖的大型粉煤灰砖厂。该厂每一昼夜能处理掉160吨粉煤灰。粉煤灰的化学成份是,SiO_2:35~45%;Al_2O_3:20~30%;Fe_2O_3·FeO:5~15%;CaO:1.5~3%;MgO:0.5~2%;SO_3:0.5~1.5%;未完全燃烧物10~15%。该厂用90%粉煤灰和10%石灰配制成砖。砖的容重为1200公斤/米~3时,其抗压强度60~100公斤/厘
The earliest industrial production of autoclaved fly ash bricks was in West Germany. In a power plant area, a large fly ash brick factory with a daily production capacity of 90,000 bricks was built. The factory can dispose of 160 tons of fly ash every day and night. The chemical composition of fly ash is: SiO_2: 35-45%; Al_2O_3: 20-30%; Fe_2O_3·FeO: 5-15%; CaO: 1.5-3%; MgO: 0.5-2%; SO3: 0.5-1.5 %; incomplete combustion 10 to 15%. The factory uses 90% fly ash and 10% lime to make bricks. When the bulk density of the brick is 1200 kg/m~3, the compressive strength is 60 to 100 kg/PCT.