华能德州电厂三期 5号锅炉 2 0 0 2年 6月 12 ,15日 2次发生包覆过热器管子爆管 ,经过第 1次改造后 ,同年8月 2 1日过热器管再次爆管。由于爆口长时间过热 ,爆口附近组织球化严重 ,包覆过热器管蠕变破坏。第 1次改造通过加装连通管 ,去除水冷壁部分卫燃带 ,刷耐热涂料 ,减少该部位的传热。第 2次改造时加装均流管 ,调整一、二、三次风旋流强度及风压等 ,降低炉膛出口烟温 ,减少减温水喷水量 ,增加包覆过热器管通流量 ,燃用接近设计煤质的煤种 ,取得了较好的效果。
Huaneng Texas Power Plant Phase III boiler No. 5 on June 12, 2002 on the 12th occurred covered tube burst pipe superheater, after the first transformation, the same year on August 21 superheater tube burst tube. Due to prolonged overheating of the pop-up, the pop-up near the ball is serious, covered superheater tube creep damage. The first transformation through the installation of connecting pipe, remove the water wall part of the health belt, brush heat-resistant paint, reducing heat transfer in this part. The second transformation of the installation of all-flow tube, adjust the cyclone intensity of the first and second, three times the wind pressure and so on, to reduce the furnace outlet temperature, reduce water spray water temperature, increase the coverage of the superheater tube flow, combustion Close to the design of coal quality coal, and achieved good results.